Metaliza SA METALIZA SA
Rotary / reciprocating compressor body
← Back to the finder

Rotary / reciprocating compressor body

Application zones

See technical detail

Resistance to abrasive sliding wear

Service life:
Repair of a used part: the performance of a thermal-sprayed part versus an original one ranges from similar (using a very basic coating material, or one equivalent to the part's original material) up to 2–10 times the service life, by applying high-performance engineering materials. Use in manufacturing: when a particular material is specified based on mechanical–chemical behavior, the component's service life is only possible if the coating is applied.
Wear agent:
Sliding of one surface over another, with wear further accelerated by airborne dust particles, impurities in lubricants, contaminants in fluids, etc.
Attack effect:
Increased roughness. As the phenomenon begins, friction coefficients rise, facilitating the abrasive effect and causing a cascading feedback that increases wear until deformation and grooves of varying depth become visible.
Layer description:
Geometrically restores the components, making them reusable. In many cases, when a packing zone separates an area with corrosive agents from an inert area, the material must be chosen according to its mechanical and chemical resistance.
Layer application:
When deformation occurs in service. During the design stage it is determined that a material better suited to this function be added during the part's manufacture.
Material type:
Steel-type metal alloys. High-chromium metal alloys. Nickel-base alloys. Cobalt-base alloys. White metal. Ceramic materials. Carbides.
Typical location:
Bearing working areas. Linear displacements.

Cavitation resistance

Service life:
Repair of a used part: the performance of a thermal-sprayed part versus an original one ranges from similar (using a very basic coating material, or one equivalent to the part's original material) up to 2–10 times the service life, by applying high-performance engineering materials. Use in manufacturing: when a particular material is specified based on mechanical–chemical behavior, the component's service life is only possible if the coating is applied.
Wear agent:
Particles traveling at high speed in fluids produce abrasive wear in line with the fluid's displacement. This can occur in liquid or gas flows.
Attack effect:
General aerodynamic deformation and/or profile change for surfaces in liquid fluids. Wall loss and consequent changes in mechanical and/or structural strength.
Layer description:
Protects the surface subjected to cavitation and extends its service life, or geometrically restores it.
Layer application:
When cavitation occurs in service. During the design stage it is determined that a material better suited to this function be added during the part's manufacture.
Material type:
High-chromium metal alloys. Nickel-base alloys. Carbides.
Typical location:
Areas exposed to erosion by particles suspended in fluids.

Sub-industries & Industries

Have a similar case?

Contact us